Most bad edges come down to four settings: gas pressure, focus position, cutting speed and nozzle condition. Each answer starts from what you see on the part (burr on the bottom edge, dross that will not knock off, deep striations, spatter, a kerf wider at the top) and goes through the causes in the order a service engineer checks them. Photos come from our defect reference. Photo diagnosis of your own part is in SBM Laser Help.
Describe the defect in your own words and SBM Laser Help smart search answers with the cause and the parameter changes.Smart search in the app →
Burr on stainless cut with nitrogen almost always means the melt is not being blown out fast enough: cutting speed too low for the power, nitrogen pressure or purity too low, a worn or off-centre nozzle, or focus sitting too high in the sheet. Start with nozzle condition and gas pressure — they explain most burr cases in a shop.
Read the answer →When a machine that used to cut through stops penetrating, the beam is losing energy on its way to the sheet or landing in the wrong place. In order of likelihood: dirty or cracked protective glass, worn nozzle, focus drift, gas pressure loss, and only then the source itself.
Read the answer →Dross on mild steel is molten oxide that solidified before the gas could remove it. The usual levers, in this order: oxygen pressure (often too high on thick plate), cutting speed, focus position, and nozzle standoff. On plate above 10 mm, most dross problems are a pressure and focus problem, not a power problem.
Read the answer →Striations are the fingerprint of an unstable melt front. Coarse, dragging lines mean the melt cannot keep up — usually speed, focus or gas dynamics. Fine even lines are normal and cannot be removed entirely; what you control is their depth and how far down the edge they start.
Read the answer →Spatter is melt ejected back up toward the head instead of down through the kerf — usually from piercing thick material too aggressively, standoff set too low, or pressure too high for the nozzle. It clogs the nozzle fast, and a clogged nozzle then makes spatter worse.
Read the answer →Taper means the beam is not delivering a straight-walled cut through the full thickness: usually focus sitting at or above the surface on thick material, speed slightly too high, or a worn lens spreading the beam. It shows up mostly on plate over 8–10 mm, where the beam has more depth to travel through.
Read the answer →SBM Laser Help carries cutting and piercing parameter tables by material, thickness and gas, photo diagnosis of cut defects, machine and chiller error codes, and gas consumption calculators. Free account, no card.